Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne Maxxam™ FR PP 307 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | ASTM D955 |
PolyOne Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ASTM D955 and ISO 294-4 |
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6
(discontinued **) Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm @Thickness 3.20 mm |
0.012 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® HV1005S PBT Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RP004 is a compound based on PA66 resin containing PTFE, Silicone. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp FF008L PE LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66 LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® 21LH-NBK4 General Purpose Nylon 66 Description: General Purpose Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | DIS 294-4 |
Wellman Wellamid® MRT1487 BK Nylon 66, 32% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ASTM D955 |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |