Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant Halogen and phosphor freeInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
Polyplastic Armlen® PP MF 40-4M Polypropylene Copolymer, 40% Calcium Carbonate High impact resistance at low temperatureInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
PolyOne Maxxam™ 34-1520 SSM TFPP Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm @Thickness 3.20 mm |
0.0070 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3300 PP+MF30% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.012 cm/cm @Thickness 3.20 mm |
0.0050 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm @Thickness 3.20 mm |
0.0060 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.012 cm/cm @Thickness 3.20 mm |
0.0050 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON PX08024 PA 6 (Europe-Africa-Middle East) LNP* STAT-KON* PX08024 is a compound based on PA 6 resin containing Mineral. Added features include; Electrically Conductive, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm @Thickness 3.20 mm |
0.0080 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.012 cm/cm @Thickness 3.20 mm |
0.0030 - 0.012 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on Tensile Bar; E2P method |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |