Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
ASTM D955
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat..
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
ASTM D955
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
LATI Latamid 12 CP/85 PA 12
Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Linear Mold Shrinkage, Flow 0.0055 - 0.0085 cm/cm
0.0055 - 0.0085 in/in
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
LATI Laticonther 83 CP/80 PA12, Impact Modified
High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Linear Mold Shrinkage, Flow 0.0055 - 0.0085 cm/cm
0.0055 - 0.0085 in/in
LATI Latimass 82-03 D080 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 771 PBT
35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing.
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm

@Thickness 3.00 mm
0.0065 - 0.0085 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® T65 AT PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm

@Thickness 3.00 mm
0.0065 - 0.0085 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® T65 HI PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature ..
Linear Mold Shrinkage, Flow 0.0045 - 0.0085 cm/cm
0.0045 - 0.0085 in/in
on Tensile Bar; ISO 294
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded
BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Linear Mold Shrinkage, Flow 0.0045 - 0.0085 cm/cm
0.0045 - 0.0085 in/in
on Tensile Bar; ISO 294
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded
BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
ASTM D955
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P..
Linear Mold Shrinkage, Flow 0.0055 - 0.0085 cm/cm
0.0055 - 0.0085 in/in
LATI Latimass 82-03 D110 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..