Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Asia Pacific) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Asia Pacific) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Lastilac 10 ABS/PC ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latilub 87/28-20T PC, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE.Information provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latistat 36/MR-04 ABS Dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0065 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.00 mm |
0.0055 - 0.0075 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.00 mm |
0.0055 - 0.0075 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® T50 BBS083 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Asia Pacific) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |