Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | ASTM D955 |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Lexan® PPC4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | SABIC Method |
SABIC Innovative Plastics LNP COLORCOMP J1000E PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000E is a compound based on PES resin. Added features include: Easy Moulding. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | ASTM D955 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm @Thickness 6.40 mm |
0.0090 - 0.011 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FL3000 PC (Asia Pacific) Structural foam: 10% weight reduction at 0.250" wall. ECO-conforming. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**) EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm @Thickness 3.20 mm |
0.0090 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm @Thickness 3.20 mm |
0.0090 - 0.013 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | |
LATI Latigray 66-01 CX/50 PA 66 Radiopaque compound based on Polyamide 66 (PA66). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP LX82803 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LX82803 is a compound based on Polyetheretherketone resin containing Proprietary Lubricant. Added features include : Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.016 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm @Thickness 3.20 mm |
0.0090 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm @Thickness 3.17 mm |
0.0090 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 AF Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedInformat.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TS271P4 PA46-MF20 20% Whisker Reinforced, Wear and Friction Modified |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm @Diameter 2.00 mm |
0.0090 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP PH0220AC PA 6 (Europe-Africa-Middle East) LNP* Thermocomp* PH0220AC is a compound based on Nylon 6 resin containing High Specific Gravity Filler. |