Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | |
Polycasa Acryl® KR 2007/1 Acrylic Medium stiffness impact grade with good heat distortion resistance. Can be extruded to thin tubes and profile and film. Easy to vacuum form. Lamp covers, cable boxes.Data was collected by ISO met.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | |
Polycasa Acryl® G 88 E Acrylic Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs .. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | |
Polycasa Acryl® KR 2010/1 Acrylic, Impact Grade High-impact grade with good flowability (e.g. for lamp covers).Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | Injection molding; ISO 2577 |
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive
(discontinued **) Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
LATI Latamid 12 CP/85 PA 12 Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0073 cm/cm @Thickness 3.20 mm |
0.0065 - 0.0073 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0073 cm/cm @Thickness 3.20 mm |
0.0065 - 0.0073 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0065 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm @Thickness 3.00 mm |
0.0065 - 0.0085 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm | 0.0065 in/in | b.o. ISO 2577 |
Covestro Makroblend® UT305 PC/PET Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• High moisture en.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Linear Mold Shrinkage, Flow | 0.0065 cm/cm @Thickness 2.00 mm |
0.0065 in/in @Thickness 0.0787 in |
60x60x2 mm; 500 bar; ISO 294-4 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |