Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | SABIC Method |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latiohm 87/28-07 CNT PC Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0070 cm/cm | 0.0055 - 0.0070 in/in | |
LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Compression molding; ISO 2577 |
Hexion Keripol® RZ 1141 Polyester Molding Compound, High Surface Quality Polyester molding compound, organically/inorganically filled, glass fiber reinforced, styrene free, very slight post shrinkage, processing shrinkage as for phenolic molding compounds, high surface q.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF14 L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF15 HS L BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF15 UV002 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: UV Stabilizer and LubricantFeatures: Good UV Resistance and LubricatedInforma.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |