Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.00010 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow <= 0.00010 cm/cm
<= 0.00010 in/in
ASTM D955
PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI
LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.00010 - 0.00030 cm/cm

@Time 86400 sec
0.00010 - 0.00030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
Linear Mold Shrinkage, Flow 0.00010 - 0.00030 cm/cm

@Time 86400 sec
0.00010 - 0.00030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0069F PC
LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding.
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide
Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI
LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow.
Linear Mold Shrinkage, Flow 0.00010 - 0.00050 cm/cm

@Time 86400 sec
0.00010 - 0.00050 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI
LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing
Linear Mold Shrinkage, Flow 0.00010 - 0.00030 cm/cm

@Time 86400 sec
0.00010 - 0.00030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES
LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.00010 cm/cm
0.00010 in/in
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic..
Copyright © lookpolymers.com All Rights Reserved