Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.025 - 0.028 cm/cm | 0.025 - 0.028 in/in | ASTM D955 |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.028 cm/cm | 0.024 - 0.028 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East) LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.026 - 0.028 cm/cm @Time 86400 sec |
0.026 - 0.028 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.028 cm/cm | 0.018 - 0.028 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.028 cm/cm | 0.018 - 0.028 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Linear Mold Shrinkage, Flow | 0.024 - 0.028 cm/cm | 0.024 - 0.028 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.026 - 0.028 cm/cm @Thickness 4.00 mm |
0.026 - 0.028 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D61 POM, Injection Molded Star L POM D61 is a PTFE/Silicone Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |