Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.018 - 0.024 cm/cm | 0.018 - 0.024 in/in | ASTM D955 |
PolyOne Nymax™ 1200 A UV White 205 Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm | 0.021 - 0.024 in/in | |
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.024 cm/cm @Thickness 3.20 mm |
0.016 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.024 cm/cm @Thickness 3.20 mm |
0.016 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.024 cm/cm @Thickness 3.20 mm |
0.019 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.024 cm/cm @Thickness 3.20 mm |
0.016 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.024 cm/cm | 0.020 - 0.024 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22L-NBK1 Engineering Grade Nylon 66 Description: Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.024 cm/cm | 0.020 - 0.024 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1627-WBK2 High Impact, Weatherable Nylon 66 Description: High Impact, Weatherable Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2880L Thermoplastic Elastomer Elastocon® 2880L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2880L is FDA compliant and well s.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.024 cm/cm | 0.020 - 0.024 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOTUF W1000I PBT (Europe-Africa-Middle East) LNP* THERMOTUF* W1000I is a compound based on Polybutylene Terephalate resin. Added features include: High Impact |