Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 2.00 mm, Temperature 23.0 °C |
0.015 - 0.019 in/in @Thickness 0.0787 in, Temperature 73.4 °F |
Internal Method |
PolyOne OnFlex™ HT 70A-3S2103 Thermoplastic Elastomer (TPE) OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6 Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.019 cm/cm @Thickness 3.17 mm |
0.014 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B70CA Polyvinyl Chloride, Flexible (PVC, Flexible) Improved adhesion.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B70CB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.019 cm/cm | 0.011 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.20 mm |
0.015 - 0.019 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.20 mm |
0.015 - 0.019 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.019 cm/cm | 0.016 - 0.019 in/in | |
LATI Latigray 75/4-01 CX/45 PBT Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L.. |
|||
Linear Mold Shrinkage, Flow | 0.0155 - 0.019 cm/cm | 0.0155 - 0.019 in/in | |
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.019 cm/cm | 0.0060 - 0.019 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.019 cm/cm | 0.0060 - 0.019 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | DIS 294-4 |
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |