Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.17 mm |
0.012 - 0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 7700 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm | 0.0090 - 0.016 in/in | ASTM D955 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | ASTM D955 |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 3.20 mm |
0.0090 - 0.016 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.016 cm/cm | 0.011 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East) LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.016 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.016 cm/cm @Thickness 0.750 - 2.30 mm |
0.0090 - 0.016 in/in @Thickness 0.0295 - 0.0906 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.016 cm/cm @Thickness 3.20 mm |
0.0060 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP PB006SXS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PB006SXS is a compound based on PA 6 resin containing Glass Bead. Added features include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East) NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 3.20 mm |
0.013 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PS+PA (Asia Pacific) High flow NORYL GTX resin for under-the-hood and electrical applications requiring retention of properties under thermal load |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22L-BL Engineering Grade Nylon 66 Description: Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | DIS 294-4 |
Wellman Wellamid® 42L-XE-N Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | on Tensile Bar; E2P method |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm @Thickness 4.00 mm |
0.014 - 0.016 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm @Thickness 4.00 mm |
0.013 - 0.016 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA6 D36 PA6, Injection Molded Star L PA6 D36 is a MOS2 Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
LATI Latimass 53-04 D009 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ISO DIS 294-4 |
Wellman Wellamid® 42LH-NBK1 General Purpose Nylon 6 Description: General Purpose Nylon 6Information provided by Wellman. |