Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 940ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Lexan® FXM123R PC (Asia Pacific) FXM123R is a Lexan PC grade in Metallic or Pearlescent effects, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package .. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® IR 2210 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose grade having low levels of ionics species. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Lexan® OQ4320 PC (Europe-Africa-Middle East) LEXAN OQ4320 is a medium viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard grades. Fields of application for this material are optical lenses, f.i. in sunglas.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0070 cm/cm | 0.0055 - 0.0070 in/in | |
LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Time 86400 sec |
0.0040 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl EM6100F PPE+PS Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® CF-1050 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |