Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | |
Solvay TECHNYL® B 238 Black 21 N PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
Unitika ET2025 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 |
DSM Stanyl® TS272A1 PA46-RF Aramid fiber reinforced, Wear and Friction Modified |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190 Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. Available in Natural and Black. Natural: Designated RH190N-3; Black: Designated RH190B.Data provid.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190H Acetal General purpose reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated RH190H-.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190H Acetal General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3.. |