Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00700 cm/cm @Thickness 3.17 mm |
0.00700 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers Polysulfone PSF P170-64170 White PSU Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio.. |
|||
Linear Mold Shrinkage, Flow | 0.00700 - 0.0100 cm/cm | 0.00700 - 0.0100 in/in | Injection; ISO 2577 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |