Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0056 cm/cm @Thickness 3.18 mm |
0.0056 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Linear Mold Shrinkage, Flow | 0.0056 - 0.0063 cm/cm @Thickness 3.20 mm |
0.0056 - 0.0063 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Linear Mold Shrinkage, Flow | 0.0056 - 0.0063 cm/cm @Thickness 3.20 mm |
0.0056 - 0.0063 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Linear Mold Shrinkage, Flow | 0.0056 - 0.0063 cm/cm @Thickness 3.20 mm |
0.0056 - 0.0063 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Linear Mold Shrinkage, Flow | 0.0056 cm/cm @Thickness 3.18 mm |
0.0056 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® XT X XT 1001 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |