Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 4.04 Ã… | 4.04 Ã… | |
Mateck Barium Titanate Crystal, BaTiO3 Oxidic single crystals. Two-wave mixing coupling constant. BaTiO3 is a very unique crystal with superior photo-refractive and ferroelectric properties. MaTecK supplies both of substrate grade and ph.. |