Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.017 g/cc @Temperature 25.0 °C |
1.017 g/cc @Temperature 77.0 °F |
|
Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulati.. |
|||
Specific Gravity | 1.017 g/cc @Temperature 15.5 °C |
1.017 g/cc @Temperature 59.9 °F |
|
Indium Corp. 1072 VOC-Free Wave Solder Flux Containing Rosin Wave Solder Flux 1072 is a halide-free, VOC-free, rosin flux specifically developed for wave-soldering, surface mount, mixed technology and through-hole electronic assemblies. This unique formulati.. |