| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | STN 64 0808 |
|
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant
FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | |
|
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | STN 64 0808 |
|
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc
FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | STN 64 0808 |
|
Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization
FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | |
|
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads
FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P100-00 Polypropylene, Natural
Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P100-01 Polypropylene Homopolymer, Black
Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P250-01 Polypropylene Copolymer, Black
Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black
Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P251-00 Polypropylene Copolymer, Natural
Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P251-01 Polypropylene Copolymer, Black
Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P254-00 Polypropylene Copolymer, Natural
Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P254-01 Polypropylene Copolymer, Black
Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P256-00 Polypropylene Copolymer, Natural
Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P256-01 Polypropylene Copolymer, Black
Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P257-00 Polypropylene Copolymer, Natural
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P257-01 Polypropylene Copolymer, Black
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | |
|
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | |
|
Plastcom SLOVAMID 6 GB 30 TS PA6, 30% glass beads
FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti..
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
Adell AD-10 Nylon 66, Ultra High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Linear Mold Shrinkage | 0.0145 cm/cm | 0.0145 in/in | ASTM D955 |
|
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||