Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D955
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black
Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D955
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ATM D955
Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNT..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ISO 2577
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP
SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
Borealis Method
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D955
Plenco 6582 Phenolic, Briquette, Transfer Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ISO 2577
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App..
Linear Mold Shrinkage 0.0011 cm/cm
0.0011 in/in
ASTM D2566-69
BCC Products BC 7136 Epoxy Casting
BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con..
Linear Mold Shrinkage 0.0011 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0011 - 0.0070 in/in
<br>@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
Copyright © lookpolymers.com All Rights Reserved