Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0125 cm/cm Grade Count:219 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0350 cm/cm | 0.00400 - 0.0350 in/in | Average value: 0.0215 cm/cm Grade Count:15 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.00705 cm/cm Grade Count:50 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0350 cm/cm | 0.0100 - 0.0350 in/in | Average value: 0.0255 cm/cm Grade Count:29 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0300 cm/cm Grade Count:123 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00391 cm/cm Grade Count:183 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.0350 cm/cm | 0.000200 - 0.0350 in/in | Average value: 0.00317 cm/cm Grade Count:150 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.0350 cm/cm | 0.000200 - 0.0350 in/in | Average value: 0.00376 cm/cm Grade Count:47 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.0350 cm/cm | 0.00150 - 0.0350 in/in | Average value: 0.0158 cm/cm Grade Count:263 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.00738 cm/cm Grade Count:232 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00417 cm/cm Grade Count:497 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0350 cm/cm | 0.000100 - 0.0350 in/in | Average value: 0.0127 cm/cm Grade Count:220 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0350 cm/cm | 0.00800 - 0.0350 in/in | Average value: 0.0193 cm/cm Grade Count:33 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0350 cm/cm | 0.000300 - 0.0350 in/in | Average value: 0.00325 cm/cm Grade Count:111 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Linear Mold Shrinkage | 0.000150 - 0.0350 cm/cm | 0.000150 - 0.0350 in/in | Average value: 0.0123 cm/cm Grade Count:213 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |