Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.00 - 0.035 cm/cm | 0.00 - 0.035 in/in | ASTM 1917 |
Nitriflex SB-1009 Styrene Butadiene Copolymer Applications: Used to promote better dimensional stability in articles like profiles, hoses, shoe sole and also recommended to PSA adhesives and adhesives for vertical applications. Available in bal.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.035 cm/cm | 0.0025 - 0.035 in/in | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |