Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00500 - 0.0300 cm/cm | 0.00500 - 0.0300 in/in | Average value: 0.0112 cm/cm Grade Count:34 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0300 cm/cm | 0.00300 - 0.0300 in/in | Average value: 0.00981 cm/cm Grade Count:32 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0300 cm/cm | 0.00500 - 0.0300 in/in | Average value: 0.0160 cm/cm Grade Count:29 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0300 cm/cm | 0.00800 - 0.0300 in/in | Average value: 0.0164 cm/cm Grade Count:29 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.00641 cm/cm Grade Count:75 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.00332 cm/cm Grade Count:111 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0300 cm/cm | 0.000 - 0.0300 in/in | Average value: 0.00259 cm/cm Grade Count:88 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.0118 cm/cm Grade Count:49 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0300 cm/cm | 0.000600 - 0.0300 in/in | Average value: 0.00621 cm/cm Grade Count:175 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.00469 cm/cm Grade Count:144 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0221 cm/cm Grade Count:20 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.0150 - 0.0300 cm/cm | 0.0150 - 0.0300 in/in | Average value: 0.0176 cm/cm Grade Count:6 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.000700 - 0.0300 cm/cm | 0.000700 - 0.0300 in/in | Average value: 0.00908 cm/cm Grade Count:37 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |