Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00700 - 0.0180 cm/cm | 0.00700 - 0.0180 in/in | Average value: 0.0108 cm/cm Grade Count:24 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0180 cm/cm | 0.00300 - 0.0180 in/in | Average value: 0.0102 cm/cm Grade Count:24 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00669 cm/cm Grade Count:113 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00743 cm/cm Grade Count:56 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00226 cm/cm Grade Count:36 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00481 cm/cm Grade Count:51 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0180 cm/cm | 0.000500 - 0.0180 in/in | Average value: 0.00327 cm/cm Grade Count:31 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0180 cm/cm | 0.00400 - 0.0180 in/in | Average value: 0.0126 cm/cm Grade Count:4 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0180 cm/cm | 0.0100 - 0.0180 in/in | Average value: 0.0120 cm/cm Grade Count:33 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.0180 cm/cm | 0.00600 - 0.0180 in/in | Average value: 0.0100 cm/cm Grade Count:9 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |