Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm | 0.0080 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 W-GV25 Nylon 6.6, std. viscosity for injection molding, 25% glass fiber reinforced Nylon 6.6, std. viscosity for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.016 cm/cm | 0.0060 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8356 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon KOPA® KN173HI2 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-0856/GY7 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7018/GN PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.011 - 0.016 cm/cm @Temperature 23.0 °C |
0.011 - 0.016 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon KOPA® KN173HI3R High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Linear Mold Shrinkage | 0.011 - 0.016 cm/cm @Thickness 3.20 mm |
0.011 - 0.016 in/in @Thickness 0.126 in |
48 hr, at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ISO 2577 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.011 - 0.016 cm/cm @Thickness 3.20 mm |
0.011 - 0.016 in/in @Thickness 0.126 in |
48 hr, at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | as molded; ISO 294 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | as molded; ISO 294 |
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E.. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ISO 2577 |
Polyram RamOfin PPC104 Polypropylene Copolymer Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | |
Polyram PlusTek RB506 Nylon 6, Flame Retardant Flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |