Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00110 - 0.0150 cm/cm | 0.00110 - 0.0150 in/in | Average value: 0.00698 cm/cm Grade Count:50 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00884 cm/cm Grade Count:13 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0150 cm/cm | 0.00400 - 0.0150 in/in | Average value: 0.00667 cm/cm Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00252 cm/cm Grade Count:23 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0150 cm/cm | 0.000300 - 0.0150 in/in | Average value: 0.00402 cm/cm Grade Count:139 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.000 - 0.0150 cm/cm | 0.000 - 0.0150 in/in | Average value: 0.00533 cm/cm Grade Count:3 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.000800 - 0.0150 cm/cm | 0.000800 - 0.0150 in/in | Average value: 0.00456 cm/cm Grade Count:120 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00884 cm/cm Grade Count:25 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00466 cm/cm Grade Count:151 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00693 cm/cm Grade Count:7 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.0150 cm/cm | 0.000200 - 0.0150 in/in | Average value: 0.00252 cm/cm Grade Count:28 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00430 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00602 cm/cm Grade Count:69 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00465 cm/cm Grade Count:33 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00314 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00421 cm/cm Grade Count:132 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00625 cm/cm Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00826 cm/cm Grade Count:36 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00767 cm/cm Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00457 cm/cm Grade Count:96 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0150 cm/cm | 0.000500 - 0.0150 in/in | Average value: 0.00348 cm/cm Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |
|||
Linear Mold Shrinkage | 0.00700 - 0.0150 cm/cm | 0.00700 - 0.0150 in/in | Average value: 0.0121 cm/cm Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |