Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00618 cm/cm Grade Count:216 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0120 cm/cm | 0.00100 - 0.0120 in/in | Average value: 0.00503 cm/cm Grade Count:19 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0120 cm/cm | 0.00500 - 0.0120 in/in | Average value: 0.00800 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0120 cm/cm | 0.000500 - 0.0120 in/in | Average value: 0.00394 cm/cm Grade Count:76 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.000900 - 0.0120 cm/cm | 0.000900 - 0.0120 in/in | Average value: 0.00745 cm/cm Grade Count:41 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Linear Mold Shrinkage | 0.00830 - 0.0120 cm/cm | 0.00830 - 0.0120 in/in | Average value: 0.00953 cm/cm Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Linear Mold Shrinkage | 0.00330 - 0.0120 cm/cm | 0.00330 - 0.0120 in/in | Average value: 0.00687 cm/cm Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00350 - 0.0120 cm/cm | 0.00350 - 0.0120 in/in | Average value: 0.00708 cm/cm Grade Count:21 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00833 cm/cm Grade Count:10 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0120 cm/cm | 0.00100 - 0.0120 in/in | Average value: 0.00366 cm/cm Grade Count:16 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0120 cm/cm | 0.000 - 0.0120 in/in | Average value: 0.00205 cm/cm Grade Count:38 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00509 cm/cm Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.00150 - 0.0120 cm/cm | 0.00150 - 0.0120 in/in | Average value: 0.00433 cm/cm Grade Count:33 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0120 cm/cm | 0.000500 - 0.0120 in/in | Average value: 0.00377 cm/cm Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |