Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC T4030 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ NH6 Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ NH9L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0040 - 0.012 cm/cm | 0.0040 - 0.012 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Isotropic shrinkage characteristics.Emergency running property.Information provided by Leh.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Temperature 23.0 °C |
0.0080 - 0.012 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.012 cm/cm @Thickness 3.00 mm |
0.0020 - 0.012 in/in @Thickness 0.118 in |
ASTM D955 |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 1001 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.012 cm/cm @Thickness 3.175 mm |
0.0030 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.012 cm/cm @Thickness 3.175 mm |
0.0040 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
Polyram RamTal PM3007G2 Polyacetal for Injection Molding, 10% Glass Fiber Reinforced 10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.175 mm |
0.0080 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
Cheng Yu Plastic ML3435 PC, 35% Glass Fiber |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Internal |
Ecomass® 1007ZC85 Stainless Steel Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Poly.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 CP Nylon 6, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Buckeye Polymers BP RPP 2008 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPHC TS20040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXFLEX® 930 TPO
(discontinued **) Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact propert.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® MN201-G10 Nylon 66 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |