Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
Polykemi AB POLYabs R00 UV4 ABS, High Impact, UV Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs S00 AS UV ABS, High Flow, UV-Stabilized, Antistatic Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0030 - 0.0080 cm/cm | 0.0030 - 0.0080 in/in | ASTM D955 |
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Polymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
Polykemi AB POLYabs N00 ABS Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1013STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Temperature 23.0 °C |
0.0060 - 0.0080 in/in @Temperature 73.4 °F |
Plumb; ASTM D955 |
Kingfa JE2-R2 ABS/PBT Alloy Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
LG Chemical HI835S PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
LTL Color Compounds ColorRxâ„¢ PC-1000RX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Kostat BK-STAT 7048BK ABS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D 955 |
MRC Polymers NAXELL™ PC429MHI Polycarbonate, Impact Modified • Medium MFR• Good property retention, heat and dimensional stability• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants ca.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ISO 2577 |
Polyram PlusTek PA301G2 Nylon 6.6 for Injection Molding, 10% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 10% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ISO 2577 |
Polyram RamLloy PBB704 PC/ABS Alloy, UV Stabilized PC/ABS alloy, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | 24 hours; ASTM D-955 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Diamond Polymers ABSPC 8020 Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Diamond Polymers DIAMALOY 750 ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |