Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0030 - 0.0042 cm/cm | 0.0030 - 0.0042 in/in | IS 13411-1992 |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Linear Mold Shrinkage | 0.0022 - 0.0042 cm/cm | 0.0022 - 0.0042 in/in | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |