Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | |
Plastcom SLOVAMID 66 HI/1 TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 20 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ Electro 242-2 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FFSL 7031 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2030 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2050 Liquid Silicon Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2641 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4050 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 4670 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 7080 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT HE Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating - Physical Properties are subject to the substrate that is used. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | ASTM-D1204 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |
|||
Linear Mold Shrinkage | 0.035 cm/cm | 0.035 in/in | vulcanized 10 sec at 200°C then post-cured |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/35 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |