Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 80.0 mm |
0.022 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Kolon KOCETAL® K100 Standard Grade Acetal Resin Suitable for extrusion and injection molding of thick products. Applications: Extruded use such as rod, pipe, tube, and sheetInformation provided by API Kolon. |
|||
Linear Mold Shrinkage | 0.022 - 0.027 cm/cm | 0.022 - 0.027 in/in | ASTM D955 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-2 PP Black Polypropylene Copolymer AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A high flow polypropylene copolymer resin, pre-colored black, specifically designed for all high speed injection molding applicati.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break AAROLENE® ARPP 200-4 Series Polypropylene Compounded ResinFeatures: A copolymer polypropylene resin, pre-colored black, featuring excellent toughness for all extrusion applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Aaron Industries AVPP HOMO 200-1 Virgin Polypropylene A virgin polypropylene specifically designed for all injection molding applications. |
|||
Linear Mold Shrinkage | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, Conditioned Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite
(discontinued **) Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p.. |
|||
Linear Mold Shrinkage | 0.022 cm/cm | 0.022 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc. |