Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0127 cm/cm | 0.0127 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Linear Mold Shrinkage | 0.0127 cm/cm | 0.0127 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Linear Mold Shrinkage | 0.0127 cm/cm | 0.0127 in/in | |
Plastcom SLOVAMID 6 GF 5 PA6, 5% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 5% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and .. |
|||
Linear Mold Shrinkage | 0.0127 cm/cm | 0.0127 in/in | ASTM D955 |
PolyOne Synprene® IT 086LFR Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Flame RetardantMulti-Purpose Thermoplastic ElastomerApplications:General PurposeInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Co.. |