Linear Mold Shrinkage 0.0098 cm/cm
0.0098 in/in
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties
FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i..
Linear Mold Shrinkage 0.0098 cm/cm
0.0098 in/in
ASTM D955
Plenco 7202 Phenolic, Granular, Injection Molded
PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065..
Linear Mold Shrinkage 0.0098 cm/cm
0.0098 in/in
Cytec EN-2527 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Linear Mold Shrinkage 0.0098 cm/cm
0.0098 in/in
ASTM D955
Plenco 7579 Phenolic, Granular, Injection Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..