Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955-89 |
Multibase Multi-Flex® TPO 1047 (AH) The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPC TS8030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 HS-SG-GV2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B11^ F30 FR5 Nylon 6, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ F20 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
PolyOne Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled
(discontinued **) PRELIMINARY DATA SHEETDescription/Features:Glass Fiber ReinforcedBlackInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM Data MD |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm @Temperature 23.0 °C |
0.0090 - 0.011 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ISO 2577 |
LyondellBasell Astryn EPKC10ZC Polypropylene Copolymer, Mineral Filled Key Features: medium high melt flow, very high modulus, UV-stabilized, mineral-filled polypropylene copolymer, very high rigidity, good impact resistance, good weatherability, good processabilityApp.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.0147 cm/cm | 0.0090 - 0.0147 in/in | ASTM D955 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | average process; cross flow; 150x80x2mm |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0090 - 0.014 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0090 - 0.014 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm @Thickness 4.00 mm |
0.0090 - 0.011 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 GS 15 HWCP 15% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm @Thickness 4.00 mm |
0.0090 - 0.011 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336M10CL Mica Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Ashley Polymers Ashlene® 830LN Nylon 6 Basic Nylon 6, medium viscosity, lubricated and nucleated for injection molding.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Aaron Industries AAROPRENE® CFPP 2030 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM data MD |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Injection; ASTM D955 |
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock.. |