Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | Compression; ASTM D955 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | Compression; ASTM D955 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | RHODIA-EP |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 185A L series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 185A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® 198A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | |
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | Injection Molding; ISO 2577 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
Polyram RamTough PZ322G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | |
Polyram PlusTek RA303G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Adell AR-34 Nylon 66, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
Adell BR-14 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0045 - 0.0055 cm/cm | 0.0045 - 0.0055 in/in | IS 13411-1992 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | restricted |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |