Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
NHEP Spectron™ E5469 Nylon 66, 33% Glass Fiber Natural color. E5469 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informat.. |
|||
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | With Flow; ISO 2577 |
Polykemi AB SCANMID 6 B32^ EF F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hysun™ 693 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
LG Chemical HI835S PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | |
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0090 cm/cm @Temperature 23.0 °C |
0.0040 - 0.0090 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ASTM D 955 |
Styrolution PS 1300/1301 GPPS Profile extrusionGood balance of flow and strengthHigh stiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ISO 294 |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ISO 294 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | as molded |
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | 24 hours; ASTM D-955 |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Diamond Polymers ASAPC GLY 130 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
Diamond Polymers NPP30-0400 MGF30 30% Mineral & Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | |
E-Polymers TEKAMID® TA210SG30 Impact Modified, 30% Glass Fiber Reinforced PA66, DAM 30% Glass Fiber reinforced, Impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ISO 2577 |
Cossa Polimeri ESTABLEND PA 1616 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, good dimensional stabil.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM Data; MD |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® 301-G30RF PBT Resin 30% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D-955 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print.. |