Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | |
Ovation Polymers RIGITRON 20415 GF PBT, 15% Glass Reinforced PBT - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polycarbonate for Injection Molding 10% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm @Thickness 1.59 mm |
0.0035 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | Injection Molding; ISO 2577 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | Injection Molding; ISO 2577 |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB303G6 Nylon 6, 30% Glass Fiber 30% Glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | IS 13411-1992 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | IS 13411-1992 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | LATI |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0040 cm/cm | 0.0035 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | |
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant 15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |