Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00340 - 0.0109 cm/cm | 0.00340 - 0.0109 in/in | Average value: 0.00668 cm/cm Grade Count:31 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00340 - 0.00530 cm/cm | 0.00340 - 0.00530 in/in | Average value: 0.00430 cm/cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00340 cm/cm | 0.00340 in/in | cure shrinkage |
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound High Temperature, Low Viscosity, Low Expansion, High Glass Transition Temperature & Chemical Resistance |