Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00179 cm/cm | 0.00179 in/in | ASTM D955 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |