Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.00050 cm/cm | 0.00050 in/in | ASTM D955 |
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4084 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Linear Mold Shrinkage | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Linear Mold Shrinkage | 0.00050 cm/cm | 0.00050 in/in | ASTM D6289 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.00050 - 0.0010 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.00050 - 0.0010 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |