Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00020 - 0.0020 cm/cm @Thickness 4.00 mm |
0.00020 - 0.0020 in/in @Thickness 0.157 in |
|
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Linear Mold Shrinkage | 0.00020 - 0.0020 cm/cm @Thickness 4.00 mm |
0.00020 - 0.0020 in/in @Thickness 0.157 in |
|
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | 0.00020 cm/cm | 0.00020 in/in | Cold Part VS Cold Tool; ASTM D955 |
Applied Composites 8052 Polyester SMC Industry Application: RecreationProduct Application: Marine ProductsDistinct Features: High Strength, ResilientInformation provided by Applied Composites Corporation. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | 0.00020 - 0.0012 cm/cm | 0.00020 - 0.0012 in/in | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Linear Mold Shrinkage | 0.00020 - 0.0020 cm/cm @Thickness 4.00 mm |
0.00020 - 0.0020 in/in @Thickness 0.157 in |
|
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | <= 0.00020 cm/cm | <= 0.00020 in/in | Typical, molds cut to zero |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Linear Mold Shrinkage | 0.00020 cm/cm | 0.00020 in/in | |
Premix Premi-Glas® 7203-28 28% Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 7203-28 is a low profile, 28% glass reinforced polyester Sheet Molding Compound designed for automotive structural vehicle body panel applications that require high flexura.. |