Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00 - 0.00050 cm/cm @Thickness 3.17 mm |
0.00 - 0.00050 in/in @Thickness 0.125 in |
|
Ovation Polymers RIGITRON 30530 GF Polyester, 30% Glass Reinforced Polyester – 30 % Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Va.. |
|||
Linear Mold Shrinkage | <= 0.00 cm/cm | <= 0.00 in/in | ASTM D955 |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |
|||
Linear Mold Shrinkage | <= 0.00 cm/cm | <= 0.00 in/in | ASTM D955 |
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | ASTM D955 |
LNP Lubricomp® ECL-4036 Polyetherimide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | Ambient part /mold |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | |
Lehmann & Voss LUVOCOM® 20/XCF/30 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | |
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | ASTM D955 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0040 cm/cm | 0.00 - 0.0040 in/in | |
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber 15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.00 - 0.0050 cm/cm | 0.00 - 0.0050 in/in | |
Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber 20% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | Cold Part VS Cold Tool; ASTM D955 |
Applied Composites 8049 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: High Impact Low Profile; Paintable/In Mold Coatable; Low Shrink; Low Moisture Absorption; Bondable; Formulated for .. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | Cold Part VS Cold Tool; ASTM D955 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Linear Mold Shrinkage | 0.00 - 0.015 cm/cm | 0.00 - 0.015 in/in | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | processing; ISO 2577 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | processing; ISO 2577 |
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | |
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0010 cm/cm | 0.00 - 0.0010 in/in | Ambient part /mold |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |
|||
Linear Mold Shrinkage | 0.00 cm/cm | 0.00 in/in | shrinkage |
Rostone Rosite® 4030FS SMC Thermoset Polyester, 30% Glass Reinforced
(discontinued **) Key Features: "Zero Shrink" Grade±1/4 mil shrinkage. Provides surface smoothness for uses such as auto headlamp retainers. High impact and flexural strength combined with dimensional accuracy.Inf.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | processing; ISO 2577 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |