Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 H-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 FK 1010 Nylon 6 for injection molding, 10% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.010 - 0.017 cm/cm | 0.010 - 0.017 in/in | |
Lehmann & Voss LUVOCOM® 80-8510 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.014 - 0.017 cm/cm @Temperature 23.0 °C |
0.014 - 0.017 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA66-C111 Toughened PA66 Features:High impactLow tendency to wrapExcellent balance propertiesApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ASTM D955 |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ASTM D955 |
Kolon KOPA® KN132VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
Kolon KOPA® KN171 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5350 is an extrusion grade.Applications: Elastic threadInformation provided by Samyang. |
|||
Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |
|||
Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5450 is an extrusion grade.Information provided by Samyang. |
|||
Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ISO 2577 |
Polyram PlusTek PA803 Nylon 6.6 for Injection Molding, Impact Modified Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | ASTM D955 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | ASTM D955 |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | ASTM D955 |
Asia International Enterprise (Hong Kong) 6010FEN Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXFLEX® 930HS TPO