Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PP 1395 PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.016 cm/cm | 0.0070 - 0.016 in/in | ASTM D955 |
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm | 0.0080 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 HS-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm | 0.0080 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0070 - 0.016 cm/cm | 0.0070 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0060 - 0.016 cm/cm | 0.0060 - 0.016 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 H-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Linear Mold Shrinkage | 0.011 - 0.016 cm/cm | 0.011 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
Kolon Kopa® KN1331 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon Kopa® KN173HI Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66 Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.0080 - 0.016 cm/cm | 0.0080 - 0.016 in/in | ISO 294-4:1997 |
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | ISO 294 |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105/WT106 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-0856/GY7 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Linear Mold Shrinkage | 0.011 - 0.016 cm/cm @Thickness 3.20 mm |
0.011 - 0.016 in/in @Thickness 0.126 in |
48 hr, at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
Polyram PlusTek PB150 Nylon 6, Injection Molding Fast cycle polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
Polyram PlusTek PB840 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ISO 294-4 |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
Polyram PlusTek PB801 Nylon 6, Impact Modified impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ISO 2577 |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm @Thickness 3.17 mm |
0.014 - 0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | ASTM D955 |
Asahi Kasei Xyron® A1400 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | as molded; ISO 294 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |