Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC TS15020E Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH T20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | |
Lehmann & Voss LUVOTECH® MR 1025 BK Polyamide 66, with mineral filler Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Linear Mold Shrinkage | 0.0060 - 0.012 cm/cm @Temperature 23.0 °C |
0.0060 - 0.012 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 4112 Polyvinyl Chloride, Flexible Notes: 75°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Mold.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.012 cm/cm | 0.0020 - 0.012 in/in | ASTM D955 |
Samyang Tribit® 1501N PBT, Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1501N is a V-2 flame retardancy grade.Appli.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Techmer ES Plaslube® NY-1/MS/5 BK223 PA66 |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 1001 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 7500-90 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 3.175 mm |
0.0080 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Internal |
Ecomass® 1007TU78 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 HWUVCP Nylon 6, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 TLWCP Nylon 66, Flame Protection Grade V-2, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPHC TS15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0040 - 0.012 cm/cm @Thickness 3.175 mm |
0.0040 - 0.012 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.011 - 0.012 cm/cm | 0.011 - 0.012 in/in | |
Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled 50% mineral filled, heavy density polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |