Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.027 cm/cm @Thickness 80.0 mm |
0.027 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability) LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2003 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2030 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2070 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2560 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2670FC High Productivity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2715/50 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2735/30 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 2740 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 3786/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | vulcanized 10 sec at 200°C; Without post-cure |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Linear Mold Shrinkage | 0.027 - 0.029 cm/cm @Thickness 3.17 mm |
0.027 - 0.029 in/in @Thickness 0.125 in |
Direction of Flow; ASTM D955 |
Diamond Polymers Softflex® SF 5591 Thermoplastic Vulcanizate (TPV) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.027 cm/cm | 0.027 in/in | ASTM D955 |
PolyOne Synprene® IT 38-074 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:Hot Runner MoldingFDA (Food Contact)Teething ring & pacifierMulti-PurposeMarket:Consumer GoodsProcessing Method:I.. |