Polymer Property : Linear Mold Shrinkage = 0.0198 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0198 cm/cm
0.0198 in/in
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Linear Mold Shrinkage 0.0198 cm/cm
0.0198 in/in
Polyram RamSter PF340S6 PBT, 30% Glass Beads
30% Glass beads reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.