Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955-89 |
Multibase Multi-Pro® 0110 X Natural Polypropylene This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide.. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | |
Plastcom SLOVAMID 66 BT LS PA66, basic type FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. UV stabile. Used in automotive, electrical, engine.. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | |
Plastcom SLOVAMID 66 OB PA66, optically brightened FeaturesPA 66 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and modulus of elasticity in tension in comparison with the basic type... |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYform POM C M140 Polyoxymethylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYform POM C M140 TF2 Polyoxymethylene, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYshine PBT D201 PBT Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A53^EM Nylon 66, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ASTM D955 |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 80.0 mm |
0.018 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4406 PTFE, 60% Bronze Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Kolon KOCETAL® TF304 Wear Modified Acetal Resin PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 5003 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 3.175 mm |
0.018 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 3.175 mm |
0.018 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO 2577 |
Polyram RamTal PMH2003 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 3.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 3.175 mm |
0.018 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
CPT C-Flex® R70-005 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® SH510 Homopolymer Acetal Resin General purpose grade characterized by balanced flowability and mechanical properties.Information provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | |
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |