Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | Exxon Method |
ExxonMobil Escorene® HD-6704 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCRUses: Industrial containers, Industrial lids |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | MPC method, MD |
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
(discontinued **) TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage | <= 0.017 cm/cm | <= 0.017 in/in | Note 1 |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
SK Chemicals SKYPEL G172D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO 294-4 |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO 294-4 |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
|
Toyobo PELPRENE™ PE450B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
|
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 - 0.018 cm/cm | 0.017 - 0.018 in/in | ASTM D955 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Linear Mold Shrinkage | <= 0.017 cm/cm | <= 0.017 in/in | |
Monmouth Rubber & Plastics Durafoam™ C19XLDS EPDM Special Features: Extremely soft and conforms easily to irregular surfaces Superior buoyancy Excellent chemical resistance 100% free of HCFC & CFC Available in custom colors upon request for quoteCo.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | |
Plastcom SLOVALEN PH 21 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Linear Mold Shrinkage | 0.017 - 0.022 cm/cm | 0.017 - 0.022 in/in | ISO 294-4 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion